Step 1: decide whether it is repairable
Before anything else, check three things: whether the table base has through-cracks or severe deformation, whether the retaining ring seal has failed with signs of product leakage, and whether separator clearances have shifted because of table wear. If the base is badly deformed or cracks have propagated, overlay cannot solve it and the table must be replaced.
Step 2: solve the structural problem
The table is a thin-walled large component, so overlay heat input readily causes warping and distortion. That distorts clearance against the separator and retaining ring, causing leakage, running-off and a production drop. Mature methods include sector-based alternating deposition (dividing the table into segments welded in turn to offset thermal stress), strict interpass temperature control, rigid support or a fixture, and post-weld machining to re-align the table. These steps belong in the plan and cannot be skipped.
Step 3: material and process window
Vertical mill duty is continuous abrasion, so prioritise compression resistance, spalling resistance and high-temperature oxidation resistance. Common approaches are self-shielded open-arc wire (easy on-site application, no shielding gas) and submerged-arc wire (higher deposition efficiency, easier interpass control, better for large areas). The process window must specify preheat temperature, interpass temperature ceiling, single-pass deposition thickness, bead overlap and distortion allowance.
Why the retaining ring is often overlooked
The table retaining ring determines whether product is thrown off efficiently, and therefore drives mill output. If the outer diameter after overlay exceeds the design allowance, the ring-to-table fit changes and you get leakage or running-off. Ring repair or replacement must be planned in the same batch and the same scheme as the table overlay, not treated afterwards as a separate job.
Commissioning is the first real life test
A newly overlaid table needs a bedding-in period. During it, keep running parameters conservative (feed rate, wind speed, separator speed) to avoid shock loading an incompletely hardened overlay. Agree a commissioning plan and inspection interval with the supplier, and sample table surface hardness at 30-90 days as the basis for warranty claims.
Enquiry and sampling
Send us the duty (material type, particle size, operating temperature), liner dimensions, quantity and required delivery date in one message, and you will receive a comparable quote, a sampling plan and a selection recommendation.
Key parameters at a glance
| Parameter | Value |
|---|---|
| Standard size (mm) | 1400×3400 / 1500×3000 / 2000×3000 |
| Process | Submerged Arc Welding (SAW) |
| Type | Flux-cored wire (FCAW/SAW) |